Filling Voids and Knots With Resin
Pouring depth, sealing the void first, colour choices and why a deep pour needs more than one go.
Filling a void is the most common epoxy job on a slab, and it is a different operation from coating a top in resin. You are filling a hole, not building a surface, and the technique that makes a fill invisible is mostly about what you do before you pour.
Decide what to fill
Not every gap wants filling. A tight check that has been stable for years can be left, and a clean knot often looks better open than filled. Fill when the void is a dirt trap, when it weakens the piece, or when it will catch sleeves.
- Structural cracks want mechanical reinforcement as well as resin. See butterfly keys and crack repair.
- Through voids need a dam underneath before they can be poured.
- Bark pockets and punky wood need cleaning out to sound timber first, or the fill sits on crumbs.
What is normal in a one-piece top, and what is not, is covered in cracks, checks and voids.
Preparation decides the result
- Clean the void. Pick, brush and vacuum out loose fibre, bark and dust. A dental pick and compressed air are the two tools that make this quick.
- Dam any opening. Tape designed for the purpose on the underside, or sheet material clamped flat with a release film between. Resin finds every gap.
- Seal the walls. Brush a thin layer of the same resin into the void and let it go tacky. This stops the wood outgassing bubbles into your main pour, which is the single most common reason a fill ends up foamy.
- Warm the slab slightly. Cold wood pushes air out as it warms. Working in a stable warm room avoids a bubble front appearing hours in.
Resin cures by an exothermic reaction. Pour too deep in one go and the heat builds, which can crack the resin, scorch it, or leave it rubbery. The product data sheet gives a maximum pour depth per layer. Respect it and pour in layers, waiting for each to reach the recoat window.
Choosing a resin
Resins differ in viscosity, pot life and maximum pour depth, and the data sheet is the only reliable source for a given product. Broadly:
| Thin casting resin | Thicker table-top resin | |
|---|---|---|
| Best for | Deep voids, multiple layers | Shallow fills, surface work |
| Pour depth per layer | Greater | Smaller |
| Cure time | Slower | Faster |
| Bubble release | Good, it is thin | Needs more help |
Do not substitute one for the other because it is what is in the cupboard. A deep void poured with a fast shallow-pour product is the classic way to get a cracked, hot, cloudy fill.
Colour
- Clear reads as depth and shows every fibre inside the void. It is the most honest and the least forgiving of poor cleaning.
- Black is the safe default on walnut. It reads as shadow and hides the inside of the void completely.
- Metallic and colour are a style decision. On a one-piece slab they tend to pull attention away from the wood.
Pigment goes in by weight at the ratio the manufacturer gives. Too much pigment interferes with cure.
After the cure
Resin sands and scrapes, and it does not sand at the same rate as the wood around it, so work flat with a hard block or a card scraper rather than a soft pad which will dish the softer timber around the harder fill. Work up through the grits with the rest of the top. See the sanding sequence for a slab top.
Then finish as normal. Hardwax oil over a cured resin fill is fine and will not stick to the resin surface, which is the correct behaviour: the resin is already its own finish.
What a fill cannot do
Resin does not stop wood moving. A slab with a long filled crack will still expand and contract across its width, and a rigid fill in a moving crack can crack itself or push the wood apart elsewhere. For anything structural, the fill is cosmetic and the butterfly keys do the work.
Common questions
How deep can you pour epoxy in one go?
It depends entirely on the product. Thin casting resins allow much deeper layers than table-top resins. The data sheet gives a maximum depth per layer, and exceeding it causes heat build-up, cracking and cloudiness.
Why does my epoxy fill have bubbles?
Usually because the wood outgassed into the pour. Brush a thin seal coat into the void and let it go tacky before the main pour, and keep the slab and the room at a stable warm temperature.
Should I fill every crack in a slab?
No. Fill what is a dirt trap, a weakness or a snag. Stable tight checks and clean knots often look better left open.
Can you oil over an epoxy fill?
Yes. Sand the fill flush with the surrounding wood and finish the whole top as usual. The oil soaks into the wood and wipes off the resin, which is already its own surface.